Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 68.3 MPa | 9910 psi | 1.3 mm/min; ASTM D790 |
PolyOne LubriOne™ 5209 FPL 20 Natural Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Strength | 68.3 MPa | 9910 psi | 1.3 mm/min; ASTM D790 |
PolyOne LubriOne™ AT-000/20T Black Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Strength | 68.3 MPa | 9910 psi | ASTM D790 |
PolyOne Novablend™ 9562 Polyvinyl Chloride Alloy (PVC Alloy) Custom MoldingInformation provided by PolyOne |
|||
Flexural Strength | 68.3 MPa | 9900 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000STHL UV2 Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat StabilizedRoHS CompliantAuto Specifications: GM GMP.PA66.074 Color: BlackF.. |
|||
Flexural Strength | 68.3 MPa | 9900 psi | after 16 hours in 50°C water |
Malvern Minerals Nylon with Novakup® L-337 Silane-Treated Quartz Filler Product data demonstrates the effect of the Novakup® (lamellar quartz surface treated with A-1100) filler. A separate entry demonstrates the effect of untreated Novacite® filler in nylon. Th.. |
|||
Flexural Strength | 68.3 MPa | 9900 psi | 90°; ASTM D790 |
Zyvex Performance Materials Arovex™ 180 Carbon Nanotube Strengthened Prepreg Arovex® 180 Prepreg is a 180°F (82°C) curing carbon nanotube strengthened epoxy prepreg suitable for numerous composites applications. Arovex 180 resin contains an optimum level of carbon nanotub.. |
|||
Flexural Strength | 68.3 MPa | 9900 psi | Machine; IPC TM-650 2.4.4 |
Arlon AD1000 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards Only Woven Glass Reinforced PTFE/Ceramic with Dk of 10.2 or greaterHigh Copper Peel Strength allows for thinner etched line widthsLowest insertion loss availableLarger Panel sizes availableLow moist.. |