Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 65.0 MPa | 9430 psi | ASTM D790 |
Premix Premi-Glas® 8101 Glass Reinforced Polyester BMC Description: Premi-Glas® 8101 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex.. |
|||
Flexural Strength | <= 65.0 MPa | <= 9430 psi | ISO 178 |
Polykemi AB POLYfill PP HIP15025 HC Polypropylene Information provided by Polykemi AB |
|||
Flexural Strength | 65.0 MPa | 9430 psi | ISO 178 |
Radici Radilon® CS38 Copolyamide 6 semiaromatic Film extrusion gradeInformation provided by Radici group. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | |
Reliance Industries Polypropylene - 40% Suzorex mica (surface treated) filled Information provided by Reliance Industries |
|||
Flexural Strength | 65.0 MPa | 9430 psi | ASTM D790 |
SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS (Asia Pacific) LNP COLORCOMP* AX03654 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | ISO 178 |
Fiberfil® J-60/10/CC/30/E NATL Polypropylene Homopolymer, 10% FiberGlass and 30% Calcium Carbonate Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 65.0 MPa | 9430 psi | |
Lehmann & Voss LUVOCOM® 80/TF/18/NT Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | |
Lehmann & Voss LUVOCOM® 80-7580 Polyacetal-copolymer, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | ASTM D790 |
Kostat 7440 Conductive ABS Compound KOSTAT 7440 is a conductive thermoplastic compound based on Acrylonitrile Butadiene Styrene and a special carbon black. KOSTAT 7440 is not dependant on atmospheric conditions and is used for ESD in.. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | ASTM D790 |
Fiberfil® J-60/15/UV/HS Polypropylene Homopolymer, 15% Glass Reinforced, Heat Stabilized, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 65.0 MPa | 9430 psi | |
Lehmann & Voss LUVOCOM® 1200-7899 ABS, with steel fiber Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Isotropic shrinkage characteristics.Information provided by Lehman.. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopolymer LNP* LUBRICOMP* KP003AXZ is a compound based on Acetal Homopolymer resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP OL003A PPS - Branched LNP* LUBRICOMP* OL003A is a compound based on PPS - Branched resin containing 15% PTFE. Added features of this grade are: Wear Resistant. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | ISO 178 |
Solvay TECHNYLSTARâ„¢ S 218 MT PA6, 40% mineral filled, Conditioned Description: TechnylStar Polyamide, 40% mineral filled, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific and North AmericaProduct Appli.. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | ISO 178 |
Styrolution Luran® S 776 S Colored ASA Description: Injection molding grade with good toughness and strength. Uses include parts for garden equipment, parts for office chairs and antennas.Information provided by STYROLUTION, which is a j.. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | ISO Data |
Styrolution Terluran® GP-22 ABS Terluran GP-22 is an easy flowing grade of ABS for injection molding with high resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF and.. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | ISO Data |
Styrolution Terluran® GP-35 ABS Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an.. |
|||
Flexural Strength | 65.0 MPa @Thickness 3.20 mm |
9430 psi @Thickness 0.126 in |
3-points, 2 mm/min, Injection Molded; ISO 178 |
Styron MAGNUMâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3325 MT is a resin with excellent processing characteristics and matt surface finish. The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines.. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | ISO 178 |
Styrolution Terblend® N NM-21 XP ABS+PA (Dry) Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Flexural Strength | 65.0 MPa | 9430 psi | ISO 178 |
Styrolution Terluran® GP-25 ABS Terluran GP-25 is an easy-flow, general purpose injection molding grade with high resistance to impact and heat distortion; intended for a wide range of applications, particularly in the housings se.. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | Bending Strength |
Saint-Gobain Vitreosil® CFQ/TSC Optical Fused Quartz Vitreosil® CFQ/TSC grades are for use in less demanding applications including viewing windows for use in corrosive and high temperature environments and non-optical components such as spacers, i.. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | ASTM-D790 |
Polyram RamTal PM1409 Acetal, PTFE Filled Polyacetal filled with PTFE for sliding parts, low friction and improved wear resistance in molded parts.Information provided by Polyram Ram On Ind. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | ISO 178 |
Eastman DuraStar DS1000 Polymer, Natural Durastar DS1000 polymer has excellent appearance and clarity. Its most outstanding features are chemical resistance and excellent processing characteristics. Exposure to aromatic oils often causes c.. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | ISO 178 |
Eastman DuraStar MN610 Polymer, Natural Durastar MN610 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN610 has very .. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | ASTM D790 |
Eastman Eastar EB062 Copolyester Eastar Copolyester EB062 is a resin specifically developed for extrusion blown bottles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand. Compared to com.. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | ASTM D790 |
Eastman Provista MP002 Copolymer Provista Copolymer MP002 is a resin specifically developed for extrusion into profiles for medical applications where aesthetics such as high clarity and gloss, coupled with design flexibility and e.. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | ASTM D790 |
Eastman Provista ST Copolymer Provista Copolymer ST is a resin specifically developed for profile extrusion where high clarity and gloss, toughness, and processability are critical. Provista Copolymer ST is a second-generation m.. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | 2mm/min; ASTM D790 |
Denka TH-23 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | JIS-K-6740 |
Denka VINYKON R3105 PVC, R grade for hard extrusion A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Flexural Strength | 65.0 MPa | 9430 psi | ASTM D790 |
Aclo Accucomp Polystyrene HS0600L High Impact |