Polymer Property : Flexural Strength = 640 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 640 MPa
92800 psi
longitudinal; ISO 178
Bond Laminates TEPEX® dynalite 408-C200(2)-FG290(4)/45% Carbon – Filament Glass – TPU Consolidated Composite Laminate
Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and f..