Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 63.6 MPa | 9220 psi | ASTM D790 |
PolyOne Nanoblendâ„¢ LST 5501 Polypropylene, Unspecified (PP, Unspecified) Nanoblend compounds, formerly known as Maxxam LST, are LIGHT, STIFF AND TOUGH. Using nanoclay technology, these compounds deliver a combination of high stiffness and impact resistance to meet demand.. |
|||
Flexural Strength | 63.6 MPa | 9230 psi | ASTM D790 |
I. Stern 750 Medium Impact Black ABS Features:Easy color-abilityInjection MoldingApplicationsOffice equipmentElectronic partsSpools, ReelsInformation provided by I. Stern & Co. Inc. |