Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 57.9 MPa | 8400 psi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® FRA202 General Purpose ABS General purpose V0/5VA-rated ABSAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Strength | 57.9 MPa | 8400 psi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® FRA205 ABS Flame-retarded V0, high gloss ABS with superior UV stabilityAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Strength | 57.9 MPa | 8400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® BM-0320 J ABS, Unreinforced Heat resistantInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 57.9 MPa | 8400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® CR-0760 ABS, Unreinforced Good chemical resistanceInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 57.9 MPa | 8400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® NA-0660I ABS, Unreinforced Anti-Bacteria Grade Nano-silver high flowability antibacterial ABS that can be used in notebook keyboardsInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 57.9 MPa | 8400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SD-0150U ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 57.9 MPa @Thickness 3.17 mm |
8400 psi @Thickness 0.125 in |
ASTM D790 |
Samsung Cheil Industries Starex® SV-0167EX Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Strength | 57.9 MPa | 8400 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0857 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 57.9 MPa | 8400 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VH-0850 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 57.9 MPa | 8400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® BM-0320 J ABS, Unreinforced Heat resistantInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 57.9 MPa | 8400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® CR-0760 ABS, Unreinforced Good chemical resistanceInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 57.9 MPa | 8400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® NA-0660I ABS, Unreinforced Anti-Bacteria Grade Nano-silver high flowability antibacterial ABS that can be used in notebook keyboardsInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 57.9 MPa | 8400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SD-0150U ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 57.9 MPa @Thickness 3.17 mm |
8400 psi @Thickness 0.125 in |
ASTM D790 |
Samsung Cheil Industries Starex® SV-0167EX Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Strength | 57.9 MPa | 8400 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0857 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 57.9 MPa | 8400 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VH-0850 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 57.9 MPa | 8400 psi | ASTM D790B |
Chevron Phillips MC3700 High Flow Crystal Polystyrene DescriptionChevron polystyrene resin MC3700 crystal is a free-flowing, crystal clear polystyrene injection molding compound, designed specifically for thin- and medium-walled or long-flow, difficult.. |
|||
Flexural Strength | 57.9 MPa | 8400 psi | ASTM D790 |
Ensinger Tecatron® XP-63 Compression Molded PPS Compound, 50% Fiberglass Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Flexural Strength | 57.9 MPa | 8400 psi | ASTM D790 |
Americas Styrenics STYRON® 678D High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceExcellent clarityGood moldabilityFood Contact CompliantTypical ApplicationsDisposable cutleryHousewaresCompact disc and DVD jewel boxesDesk organizersInfor.. |