Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 53.8 MPa | 7800 psi | ASTM D790 |
Samsung Cheil Industries Starex® WR-9750 Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Strength | 53.8 MPa | 7800 psi | ASTM D790 |
Samsung Cheil Industries Starex® WR-9750 Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Strength | 53.8 MPa | 7800 psi | ASTM D790 |
Chesterton ARC HT-T Spark Testable High Temperature Trowelable Abrasion Control Compound An advanced ceramic composite formulated to protect equipment from corrosion and erosion in elevated temperature water solution immersion. This system is a high viscosity composite that is applied b.. |
|||
Flexural Strength | 53.8 MPa | 7800 psi | ASTM D-790 |
Axiall UV-6685 Rigid PVC, Molding Georgia Gulf UV 6685 is a high flow PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of parts requiring resistance to outdoor UV degradation.Info.. |
|||
Flexural Strength | 53.8 MPa | 7800 psi | Cross; IPC TM-650 2.4.4 |
Arlon CLTE-AT Commercial Ceramic PTFE Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-AT is a micro-dispersed ceramic PTFE composite utilizing .. |
|||
Flexural Strength | 53.8 - 81.4 MPa | 7800 - 11800 psi | |
Bulk Molding Compounds BMC T60 Grey Wear Resistant Molding Compound BMC T60 Grey is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu.. |
|||
Flexural Strength | 53.8 MPa | 7800 psi | |
BCC Products BC 7009-1 Epoxy Casting BC 7009-1 is an iron filled, low-cost mass casting system. Thicknesses up to two inches in non-conductive molds, and four inches in conductive molds can be achieved without foaming or yielding exces.. |
|||
Flexural Strength | 53.8 MPa | 7800 psi | ASTM D790-95 |
Multibase Multi-ABS 3075 High Impact Data provided by Multibase. |
|||
Flexural Strength | 53.8 - 81.4 MPa | 7800 - 11800 psi | |
Bulk Molding Compounds BMC T60-6006 Wear Resistant Molding Compound BMC T60-6006 is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu.. |