Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 480 MPa | 69600 psi | ASTM F417 |
CoorsTek Direct Sintered Silicon Carbide, SC DS (SC-30, UltraSiC™) Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Flexural Strength | >= 480 MPa | >= 69600 psi | high temp bending |
China-Yixing Longly Refractories Seggar SiC SiC series products of SiC shelf boards, SiC pillars, SiC slab, SiC seggar kiln furniture, are formed using high-quality silicon carbide materials and high temperature binders by tons of high-vibrat.. |
|||
Flexural Strength | >= 480 MPa | >= 69600 psi | cold bending |
China-Yixing Longly Refractories Slab SiC SiC series products of SiC shelf boards, SiC pillars, SiC slab, SiC seggar kiln furniture, are formed using high-quality silicon carbide materials and high temperature binders by tons of high-vibrat.. |
|||
Flexural Strength | >= 480 MPa | >= 69600 psi | high temp bending |
China-Yixing Longly Refractories Tube SiC SiC tube made by our company have lots of superior performance, such as high refractoriness, good wear and corrosion resistance, hardness, strength, thermal conductivity, thermal shock stability, as.. |