Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 44.8 MPa | 6500 psi | |
Ohio Carbon Blank OCB AR-06 EDM Grade Graphite Available in a range of sizes and shapes. |
|||
Flexural Strength | 44.8 MPa | 6500 psi | ASTM D790 |
Oxford Polymers PP-Homopolymer-20GF-Natural PP, 20% Glass Fiber Reinforced Product Description: Glass Fiber (20% Reinforced), Polypropylene injection molding grade Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Improved stiffnessInfor.. |
|||
Flexural Strength | 44.8 MPa | 6500 psi | ASTM D790 |
PolyOne Stat-Tech™ AS-10CP/000 Acrylonitrile Butadiene Styrene (ABS)
(discontinued **) Description/Features:AntistaticConductive Carbon Powder FilledInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 44.8 MPa | 6500 psi | ASTM D790 |
Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 44.8 MPa | 6500 psi | ASTM D790 |
I. Stern HIPS 8 High Impact Polystyrene Injection Grade Features:Good processing characteristicsComplies with FDA requirements as described in Title 21 CFR 177.1640ApplicationsDisplaysHouse waresStructural FoamInformation provided by I. Stern & Co. Inc. |
|||
Flexural Strength | 44.8 MPa | 6500 psi | ASTM D790 |
ITW Devcon Metal Repair Wear Resistant Epoxy (WR-2), Dark Grey Information provided by ITW Devcon |
|||
Flexural Strength | 44.8 MPa | 6500 psi | |
SGL Carbon Group EK 10 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Flexural Strength | 44.8 MPa | 6500 psi | |
SGL Carbon Group EK 2239 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Flexural Strength | 44.8 MPa | 6500 psi | ASTM D790 |
Techmer ES Electrafil® ABS-1200/SD/FR BL ABS |
|||
Flexural Strength | 44.8 MPa | 6500 psi | Max Load; ASTM D790 |
Spartech PE4325 Reinforced High Density Polyethylene Compound Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a.. |
|||
Flexural Strength | 44.8 MPa | 6500 psi | ASTM D 790 |
Styrolution PS 5310 HIPS Excellent ESCRGood ToughnessMatte easily decorated finishInformation provided by Styrolution |
|||
Flexural Strength | 44.8 MPa | 6500 psi | ASTM D790 |
Westlake Plastics Kynar® PVDF CN-P Polyvinylidene Fluoride (conductive) Carbon-powder-filled, thermally stable, conductive material with consistent resistivities |
|||
Flexural Strength | 44.8 MPa | 6500 psi | ASTM D790 |
Total PSI 625 Polystyrene Polystyrene 625 is a medium impact polystyrene with balanced physical properties. Thin walled parts with complex runners and gates, run fast and consistently with the easy flow 625. The natural whi.. |
|||
Flexural Strength | 44.8 MPa | 6500 psi | ASTM D790 |
Adell RQ-14 Copolymer Polypropylene, 20% Mica Reinforced Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 44.8 MPa | 6500 psi | ASTM D790 |
Asahi Kasei Thermylene® F6-10FG-0100 10% Glass Fiber Reinforced, Chemically Coupled Information provided by Asahi Thermofil |
|||
Flexural Strength | 44.8 MPa | 6500 psi | |
BCC Products BC 6126 Epoxy Surface Coat/Casting BC 6126 is a gray, low toxicity, aluminum filled, epoxy surface coat. This thixotropic resin system provides excellent surface duplication along with vertical coverage to 1/16 inch thickness. This h.. |
|||
Flexural Strength | 44.8 MPa | 6500 psi | ASTM D790 |
Asahi Kasei Thermofil P-40TC-2767 40% Talc Reinforced, Heat Stabilized Information provided by Asahi Thermofil |