Polymer Property : Flexural Strength = 38.99 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 38.99 MPa
5655 psi
s.d. 1.29 MPa, specimen 2.47 cm wide (s.d. 0.02 cm), 0.20 cm thick (s.d.008 cm), 3.8 cm span (s.d. 0 cm). Test conditions: Humidity 50%, Temp. 23°C.
Schmelzer Industries Pearlveil 110-30 Fiberglass Veil
Economical alternative for flat or shallow applications. Suitable for hand lay-up, pre-form molding, press molding, vacuum molding, and injection molding. Data provided by the manufacturer, Schmel..