Polymer Property : Flexural Strength = 38.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 38.2 MPa
5540 psi
ASTM D790
Mitsui TPX® MBZ230 Methylpentene Copolymer, Filled, Opaque Grade  (discontinued **)
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..