Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 370 MPa | 53700 psi | ISO 178 |
Solvay Specialty Polymers Amodel® DW-1140 Polyphthalamide (PPA)
(Unverified Data**) Amodel DW-1140 is a 40% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of th.. |
|||
Flexural Strength | 370 MPa | 53700 psi | |
Lehmann & Voss LUVOCOM® 1105-8417 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Flexural Strength | 370 MPa | 53700 psi | |
Lehmann & Voss LUVOCOM® 1-RG 2 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Flexural Strength | 370 MPa | 53700 psi | |
Lehmann & Voss LUVOCOM® 204-8468 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Flexural Strength | 370 MPa | 53700 psi | |
Lehmann & Voss LUVOCOM® 20-8302 Polyphthalamide, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Flexural Strength | 370 MPa | 53700 psi | ISO 178 |
Kuraray Genestarâ„¢ G1500A-M61 Nylon, 50% Glass Filled 50% Glass reinforced injection grade. Main Features:High strengthHeat resistanceExamples of applications:Structural partsSteel alternating parts |
|||
Flexural Strength | 370 MPa | 53700 psi | ISO 178 |
Kuraray Genestarâ„¢ GX1500A-M41 Nylon, 50% Glass Filled 50% Glass reinforced injection grade. This grade was developed specifically for high mechanical properties for TD direction.Main Features:Low warpageHigh mechanical properties for TD directionExamp.. |
|||
Flexural Strength | 370 MPa | 53700 psi | |
Lehmann & Voss LUVOCOM® 1105/CF/30/EM PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Flexural Strength | 370 MPa | 53700 psi | |
Lehmann & Voss LUVOCOM® 1105/XCF/15-S PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Flexural Strength | 370 MPa | 53700 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP VERTON RV00AE PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AE is a compound based on PA 66 rsin containing Long Glass Fiber. Added features include; Easy Molding. |
|||
Flexural Strength | 370 MPa | 53700 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Asia Pacific) LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Flexural Strength | 370 MPa | 53700 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Europe-Africa-Middle East) LNP VERTON* RV00AES is a compound based on PA 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Flexural Strength | 370 MPa | 53700 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP VERTON RV00AESC PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AESC is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, Heat Stabilized. |
|||
Flexural Strength | 370 MPa | 53700 psi | ISO 178 |
Unitika E-RUNG60 PA66, 60% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Flexural Strength | 370 MPa | 53700 psi | dry; ISO 178 |
DSM Novamid® 1015G50 NA/BK37 PA6-GF50 50% Glass Reinforced, Injection Molding |
|||
Flexural Strength | 370 MPa | 53700 psi | longitudinal; ISO 178 |
Bond Laminates TEPEX® dynalite 104-RG600(x)/47% Roving Glass – PP Consolidated Composite Laminate Within the TEPEX® composite laminate, PP is a resin known for its good hardness, stiffness, abrasion resistance and chemical resistance.Typical application environments are within automotive applic.. |
|||
Flexural Strength | 370 MPa | 53700 psi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Dry, 60% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Flexural Strength | 370 MPa @Temperature -40.0 °C |
53700 psi @Temperature -40.0 °F |
ASTM Test |
BASF Petra® 140 45% Glass Filled PET Petra 140 is a 45% glass reinforced injection molding polyethylene terephthalate (PET) offering an increased level of strength, stiffness, high temperature performance and dimensional stability. Ex.. |
|||
Flexural Strength | 370 MPa | 53700 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Flexural Strength | 370 MPa | 53700 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON RX06422 PA 66 LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural. |
|||
Flexural Strength | 370 MPa | 53700 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON RX06422 PA 66 (Asia Pacific) LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |