Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 37.2 MPa | 5400 psi | ASTM D790-95 |
Multibase Multi-Pro® 0110 X Natural Polypropylene This product is suitable for moldings incorporating high temperature requirements. This material is specially formulated to be resistant to Copper, but is also resistant to most metals.Data provide.. |
|||
Flexural Strength | 37.2 MPa | 5400 psi | ASTM D790 |
PolyOne Stat-Tech™ ST5220-0004 CP4D EG Black Polypropylene Impact Copolymer (PP Impact Copolymer) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Flexural Strength | 37.2 MPa | 5400 psi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers SBS 1000 Clear Styrene Butadiene Copolymer Description: Clear Styrene Butadiene CopolymerInformation provided by Network Polymers Inc. |
|||
Flexural Strength | 37.2 MPa | 5400 psi | ASTM D790 |
PolyOne Maxxam™ FR PP 301 EXT Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Flexural Strength | 37.2 MPa | 5400 psi | ASTM D790 |
PolyOne Lubri-Tech™ AS-10GB/02S Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
(discontinued **)< Description/Features:Glass Bead FilledSilicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 37.2 MPa | 5400 psi | ASTM D790 |
Fiberfil® PP-61/TC/20/UV Polypropylene Copolymer, 20% Talc, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 37.2 MPa | 5400 psi | ASTM D 790 |
Styrolution Clearblend 165 MBS CLEARBLEND 165 is an impact modified styrene acrylic copolymer blend with excellent clarity and outstanding toughness.Exceptional toughnessLow densityEase of processingLow moisture absorptionInforma.. |
|||
Flexural Strength | 37.2 MPa @Thickness 3.20 mm |
5400 psi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 556 Flame Retardant Polystyrene Characteristics Good flow properties Good balance of toughness and rigidity Available in any color Processing Extrusion MoldingApplications T.V. Cabinets, computer monitor, printer housing Elect.. |
|||
Flexural Strength | 37.2 MPa | 5400 psi | ASTM D790 |
Chase Plastics CP Pryme® NN300HSL (COND, 50% RH) Nylon 66 (Utility Grade), Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 37.2 MPa | 5400 psi | ASTM D790 |
Chase Plastics CP Pryme® NN300L (COND, 50% RH) Nylon 66 (Utility Grade), Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 37.2 MPa | 5400 psi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers SBS 1031 Clear Styrene Butadiene Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Strength | 37.2 MPa | 5400 psi | ASTM D790 |
Americas Styrenics STYRON A-TECH® 1260 High Impact Polystyrene Product CharacteristicsGood Environmental Stress Crack Resistance (ESCR)Good practical toughnessDeep draw thermoforming capableGood low temperature impactFood Contact CompliantTypical ApplicationsPa.. |
|||
Flexural Strength | 37.2 MPa | 5400 psi | |
Anderman Ceramics EM60P Sillimanite Porous synthetic mullite with high thermal shock. Available as tube up to 10 ft (3 m) long with diameters 0.6" to 2.4".Information provided by Anderman Ceramics. |
|||
Flexural Strength | 37.2 MPa | 5400 psi | ASTM D790 |
Adell EZ-18 Homopolymer Polypropylene, 40% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 37.2 MPa | 5400 psi | ASTM D790 |
Adell RA-16 Copolymer Polypropylene, 30% Talc Filled Data provided by Adell Plastics, Inc. |