Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 338 MPa | 49000 psi | ASTM D-790 |
PlastiComp Complet® LCF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Flexural Strength | 338 MPa | 49000 psi | ASTM D790 |
Oxford Polymers PEEK-20CF-Black PEEK, 20% Carbon Fiber Reinforced Product Description: Carbon Fiber (20% Reinforced), PEEK, Polyetheretherketone, injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Carbon fiber Special Ch.. |
|||
Flexural Strength | 338 MPa | 49000 psi | ASTM D790 |
LNP Thermocomp® LC-1006 EM Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Flexural Strength | 338 MPa | 49000 psi | ASTM D790 |
Techmer ES HiFill® HTN GF HS L High Temp Nylon 50% Glass Filled Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Heat ResistanceInformation provided by TP Composit.. |
|||
Flexural Strength | 338 MPa | 49000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF60 L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Compo.. |
|||
Flexural Strength | 338 MPa | 49000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF40 HS L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformati.. |
|||
Flexural Strength | 338 MPa | 49000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF40 HS L BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Flexural Strength | 338 MPa | 49000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF40 UV L BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceAppearan.. |
|||
Flexural Strength | 338 MPa | 49000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP UF00BAS PPA LNP* THERMOCOMP* UF00BAS is a compound based on Polyphthalamide containing 55% Glass Fiber. Added feature of this material is: Heat Stabilized. |
|||
Flexural Strength | 338 MPa | 49000 psi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF40 FR HS L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform.. |
|||
Flexural Strength | 338 MPa | 49000 psi | ASTM D790 |
Lubrizol Isoplast® 202LGF40 Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Flexural Strength | 338 MPa | 49000 psi | ASTM F417 |
CoorsTek AD-90 Alumina (nom. 90% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |