Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 317 MPa | 46000 psi | ASTM D790 |
PolyOne Edgetek® NN-50GF/000 Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Strength | 317 MPa | 46000 psi | ASTM D790 |
PolyOne Edgetek® NN-50GF/000EM L Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Flexural Strength | 317 MPa | 46000 psi | ASTM D790 |
PolyOne Nymax™ GF 1200 A 55 HS Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Flexural Strength | 317 MPa | 46000 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
Flexural Strength | 317 MPa | 46000 psi | ASTM D-790 |
PlastiComp Complet® LGF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 40% long glass fiber reinforcementInformation provided by Plas.. |
|||
Flexural Strength | 317 MPa | 46000 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope.. |
|||
Flexural Strength | 317 MPa | 46000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP LCL36E PEEK (Europe-Africa-Middle East) LNP* LUBRICOMP* LCL36E is a compound based on Polyetheretherketone resin containing Carbon Fiber , PTFE. Added features include : Electrically Conductive, Internally Lubricated, Easy Molding. |
|||
Flexural Strength | 317 MPa | 46000 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high .. |
|||
Flexural Strength | 317 MPa | 46000 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanic.. |
|||
Flexural Strength | 317 MPa | 46000 psi | ASTM D790 |
Techmer ES HiFill® PA4/6 GF45 HS BK 45% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackTPCI# 9627150Informat.. |
|||
Flexural Strength | 317 MPa | 46000 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66 LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b.. |
|||
Flexural Strength | 317 MPa | 46000 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Flexural Strength | 317 MPa | 46000 psi | ASTM D790 |
Techmer ES HiFill® PA4/6 GF40 HS 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedTPCI# 9627150Information provided by T.. |
|||
Flexural Strength | 317 MPa | 46000 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON RX89047 PA 66 LNP* VERTON* RX89047 is a compound based on Nylon 66 resin containing Proprietary Fillers. Added feature of this grade is: Structural. |
|||
Flexural Strength | 317 MPa | 46000 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON RX89047 PA 66 (Asia Pacific) LNP* Verton* RX89047 is a compound based on Nylon 66 resin. |
|||
Flexural Strength | 317 MPa | 46000 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON RX89047 PA 66 (Europe-Africa-Middle East) LNP* Verton* RX89047 is a compound based on Nylon 66 resin. |
|||
Flexural Strength | 317 MPa | 46000 psi | 2 mm/min; ISO 178 |
Sax Polymers SAXAMID 126F9 Nylon 6, 45% Glass Fiber SAXAMID 126F9 is a polyamide 6 injection-molding-grade reinforced with 45% glass fibers.Information provided by SAX Polymers |
|||
Flexural Strength | 317 MPa | 46000 psi | ASTM D790 |
Lubrizol Isoplast® 101LGF60BLK Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Flexural Strength | 317 MPa | 46000 psi | ASTM D790 |
Chase Plastics CP Pryme® NN143GL (DAM) Nylon 66, 43% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 317 MPa | 46000 psi | |
Aremco AREMCOLOX™ 502-1400 (Full-Fired) Dense Alumina Parts fabricated to print. Excellent physical properties and corrosion resistance. For pump liners, nozzles, guides. Standard crucibles and bolts, nuts and washers from 4-40 to 1/4-20. |
|||
Flexural Strength | 317 MPa | 46000 psi | ASTM D790 |
PolyOne Edgetek® NL-30CF/000 Nylon 6/12, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 317 MPa | 46000 psi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF50 FR UV X BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 50% Filler by WeightAdditive: Flame Retardant and UV StabilizerFeatures: Flame RetardantAppearance: BlackProcessing Method.. |