Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 31.88 MPa | 4624 psi | |
Shinil Chemical SHINNANO PP Polymer Nanocomposite IP SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |