Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 30.0 MPa | 4350 psi | |
Plastcom SLOVALEN PC 78 FRT 5 PP, glass fibre, mod. of mech. properties FeaturesModified copolymer PP for injection moulding, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Increased strength in comparison with unfilled.. |
|||
Flexural Strength | 30.0 - 40.0 MPa | 4350 - 5800 psi | ASTM D790-03 |
Proto3000 Objet DurusWhite FullCure430 Polypropylene-like Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Radici Radilon® SLVHPL128 (dry) Nylon 6 Plasticized for improved flexibilityInformation provided by Radici group. |
|||
Flexural Strength | 30.0 - 60.0 MPa | 4350 - 8700 psi | ASTM D790 |
Raschig Group PiMC 1241 Sanitary, uni color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Flexural Strength | 30.0 - 60.0 MPa | 4350 - 8700 psi | ASTM D790 |
Raschig Group PiMC 1949 Granite colors PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Flexural Strength | 30.0 MPa @Temperature 65.0 °C |
4350 psi @Temperature 149 °F |
ASTM D790 |
BASF Capron® 8200 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | |
Lehmann & Voss LUVOCOM® 65-8498 PP-copolymer, unreinforced Applications: Office communication.Reduced moment of inertia compared with metal parts.Dynamic stressed parts.Especially suitable for thin wall complex parts.Information provided by Lehmann & Voss &.. |
|||
Flexural Strength | 30.0 MPa @Temperature 22.0 °C |
4350 psi @Temperature 71.6 °F |
25 mm wide 100 mm long, flat samples; ISO 14125 |
Menzolit Menzolit® MMC 1600 Unsaturated Polyester UP MMC 1600 is a mineral moulding compound (similar to DMC/BMC) providing of a stone like appearance eg. granite or marble. Chrome plated mould surfaces are required. It is recommended that product thi.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
MRC Polymers MAXTEL™ 640-BK Polypropylene Copolymer • For extrusion or injection molding• Excellent process ability.Information provided by MRC Polymers Inc. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
Kostat E-3007J Conductive PS Compound KOSTAT E-3007J is a conductive thermoplastic compound based on impact modified polystyrene and a special conductive carbon black.KOSTAT E-3007J is not dependant on atmospheric conditions.Special Fea.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON FD000 PE LNP* STAT-KON* FD000 is an unfilled Polyethylene. Added feature of this grade is: Electrically Conductive. |
|||
Flexural Strength | 30.0 MPa @Temperature 23.0 °C |
4350 psi @Temperature 73.4 °F |
2mm/min; 80x10x4mm; ISO 178 |
SYNTHOS Krasten® FB28 High Impact Polystyrene And Polyethylene Blend Polymer blend HIPS/PE. High toughness, very good tensile properties and environmental stress cracking resistance. Processed mainly by extrusion and thermoforming. Production of sheets and films, tec.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Borealis Daplen™ EE158AI Polypropylene TPO Compound Daplen™ EE158AI is a 13% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3707 CAC03 Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 3707 is a 20% CAC03 filled homopolymer polypropylene product.Information provided by A. Schulman. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Polyram RamShine PS580 High Impact Polystyrene, Flame Retardant Flame retardant V-0, high impact polystyrene for injection molding applications.Information provided by Polyram. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
A. Schulman POLYFORT™ PP 3702 Clarified Copolymer Polypropylene DescriptionPolyfort® PP 3702 is a clarified copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | GB/9341 |
Zhejiang Juner JEPP2007 PP For Automotive Parts Applications: Inner Decorate PartsInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
A. Schulman POLYFORT™ PP 3702 Clarified Copolymer Polypropylene DescriptionPolyfort® PP 3702 is a clarified copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
A. Schulman POLYFORT™ PP 3702 Clarified Copolymer Polypropylene DescriptionPolyfort® PP 3702 is a clarified copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Borealis Daplen™ EE188AI Polypropylene TPO Compound Daplen™ EE188AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | high temp bending |
China-Yixing Longly Refractories Seggar Corundum-Mullite Our company's production of a variety of corundum mullite push slab (moved plate), corundum-mullite seggar, corundum mullite corrugated board and other kinds of the kiln furniture, high refractorine.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM D790 |
Aclo Accucomp Polypropylene CPO402V Automotive Approved Copolymer Extrusion Grade |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, Conditioned Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, Conditioned Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Flexural Strength | 30.0 MPa @Temperature 65.0 °C |
4350 psi @Temperature 149 °F |
ASTM Test |
BASF Ultramid® 8202 HS PA6 (Dry) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
Flexural Strength | 30.0 MPa @Temperature 65.0 °C |
4350 psi @Temperature 149 °F |
ASTM Test |
BASF Ultramid® 8270 HS PA6 (Dry) Ultramid 8270 HS is a thermally modified PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile extrusion, and other applications requi.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ASTM Test |
BASF Ultramid® 8350 HS PA6 (Conditioned) Ultramid 8350 HS is a heat stabilized, impact modified type 6 graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness combined with a moderate.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, Conditioned Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, .. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
BASF Nypel® 2351 HS BK PA6 (Dry) Description: Nypel® 2351 HS BK is a heat stabilized, pigmented black, impact modified PA6 extrusion grade compound. Quality and performance are combines at a lower cost. It is based on recycled PA6.. |
|||
Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 |
Polyram RamOfin PPC343T4 Polypropylene, 20% Mineral Filled 20% Mineral filled, UV stabilized, heat stabilized polypropylene for injection molding applications.Information provided by Polyram. |