Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 290 MPa | 42100 psi | |
Plastcom SLOVAMID 66 GF 40 PA66, 40% glass fibre FeaturesChemically reinforced with 40% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Flexural Strength | 290 MPa | 42100 psi | ASTM D790 |
Niche Polymer PA66GF43BK Nylon 66, 43% Glass Fiber Filled Information provided by Niche Polymer |
|||
Flexural Strength | <= 290 MPa | <= 42100 psi | ISO 178 |
Polykemi AB SCANMID 6 B12^ F50 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
Polymer Resources NY6-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
DSM Akulon® Ultraflow™ K-FHG7 Nylon 6-35% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Flexural Strength | 290 MPa | 42100 psi | |
Lehmann & Voss LUVOCOM® 1-8070 VP Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Flexural Strength | 290 MPa | 42100 psi | |
Lehmann & Voss LUVOCOM® 1-8521 Polyamide 66, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Flexural Strength | 290 MPa | 42100 psi | |
Lehmann & Voss LUVOCOM® 7-0755 Polyamide 610, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.Improved friction and wear behaviou.. |
|||
Flexural Strength | 290 MPa | 42100 psi | |
Lehmann & Voss LUVOCOM® 1-0889-5 Polyamide 66, with carbon fiber and glass fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Flexural Strength | 290 MPa | 42100 psi | |
Lehmann & Voss LUVOCOM® 1-0890 Polyamide 66, with carbon fiber, low-warpage, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c.. |
|||
Flexural Strength | 290 MPa | 42100 psi | ASTM D790 |
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Flexural Strength | 290 MPa | 42000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 HS L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizerInformati.. |
|||
Flexural Strength | 290 MPa | 42100 psi | ASTM-D790 |
Polyram Polytron A30B02 Nylon 66, 30% Long Fiber 30% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Flexural Strength | 290 MPa | 42100 psi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® FGFE5171 NC010C Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66 with Developed for Food Contact ApplicationsZytel FGFE5171 NC010C is a 33% glass filled nylon 66 resin. It has been developed for consideration into applications su.. |
|||
Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
BASF Ultramid® 8234G HS BK 102 44% Glass Filled PA6 (Dry) Description Ultramid 8234G HS BK-102 is heat stabilized, pigmented black, 44% glass reinforced PA6 injection molding compound offering the highest level of strength, stiffness, high temperature perf.. |
|||
Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H01 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Flexural Strength | 290 MPa @Temperature 23.0 °C |
42100 psi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® FGFE5171 NC010C Nylon 66
(Unverified Data**) Zytel® FGFE5171 NC010C is a 33% glass filled nylon 66 resin. It has been developed for consideration into applications such as parts for the food industry.Information provided by DuPont Performance.. |
|||
Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
Ascend Performance Materials Vydyne® R533H BK02 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK02 is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when exposed to anti-f.. |
|||
Flexural Strength | 290 MPa | 42100 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |