Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 241 MPa | 35000 psi | ASTM D790 |
PolyOne Nymax™ GF 600 A 33 HS7 DX9 Black Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Flexural Strength | 241 MPa | 35000 psi | ASTM D790 |
PolyOne Nymax™ GF 600 A 33 Natural Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Flexural Strength | 241 MPa | 35000 psi | Transverse Rupture |
PSM Industries Pacific Sintered Metals Bronze BT-121-R Powdered Metal Structural and bearing bronze Equivalent MPIF Specification: CT-1000-K23Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Flexural Strength | 241 MPa | 35000 psi | ASTM D790 |
PolyOne LubriOne™ PC-30CF/20T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Strength | 241 MPa | 35000 psi | ASTM D790 |
PolyOne Edgetek® PS-30CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 241 MPa | 35000 psi | ASTM D790 |
LNP Stat-Kon® PDX-E-99689 CCS Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued.. |
|||
Flexural Strength | 241 MPa | 35000 psi | 73°F; ASTM D790 |
Ravago Manufacturing Americas Hylon® N1035HLHR Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Flexural Strength | 241 MPa | 35000 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2400 PEI (Asia Pacific) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. WRAS certification in recognized colors. |
|||
Flexural Strength | 241 MPa | 35000 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2410R PEI (Asia Pacific) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Flexural Strength | 241 MPa | 35000 psi | ASTM D790 |
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111 is a natural-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outstanding chemical.. |
|||
Flexural Strength | 241 MPa | 35000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 IM2 L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact Modified and LubricantFeatures: Impact Modified and LubricatedProcessin.. |
|||
Flexural Strength | 241 MPa | 35000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF60 IM HS L 60% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Flexural Strength | 241 MPa | 35000 psi | ASTM D790 |
Teknor Apex Chemlon® 233 GH Nylon, 6, 30% Short Glass Fiber Reinforced Features: Good Dimensional Stability; Good Impact Resistance; Good Processability; Good Toughness; Heat Stabilized; High Strength; Lubricated Processing Method: Injection Molding Forms: Pellets Addi.. |
|||
Flexural Strength | 241 MPa | 35000 psi | ASTM D790 |
Teknor Apex Chemlon® 340G Nylon 610, Glass Fiber Reinforced Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Flexural Strength | 241 MPa | 35000 psi | ASTM D790 |
A. Schulman SCHULADUR® A GF50 50% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Strength | 241 MPa | 35000 psi | ASTM Test |
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry) Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a
balance of st.. |
|||
Flexural Strength | 241 MPa | 35000 psi | Lengthwise; ASTM D790 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Flexural Strength | 241 MPa | 35000 psi | Lengthwise; ASTM D790 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet 1/8" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Flexural Strength | 241 MPa | 35000 psi | ASTM D-790 |
PlastiComp Complet® LCF30-PC/ABS Polycarbonate/ABS Alloy, 30% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polycarbonate/ABS Alloy with 30% long carbon fiber reinforcementInformation provided b.. |