Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 221 MPa | 32100 psi | ASTM D-790 |
PlastiComp Complet® LGF30-PBT Polybutylene Terephthalate, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polybutylene Terephthalate (PBT) with 30% long glass fiber reinforcementInformation pr.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Oxford Polymers PPS/66-505-40GF-BK PPS/PA66, 40% Glass Fiber Reinforced Product Description: Glass Fiber (40% Reinforced), Polyphenylene sulfide injection molding grade based alloy with Nylon 66 Processing and Delivery Form: Pellets and Injection MoldingAppearance: Bla.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced Polyetherimide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D-790 |
PlastiComp Complet® LGF20 - TPU Rigid Thermoplastic Polyurethane, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
PolyOne Edgetek® PK-20GF/000 Polyetheretherketone (PEEK), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 (CTI Testing)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES Electrafil® J-1305/CF/30/TF/15 BK PPS |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF/M40 HS L 40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedTPCI# 7395102Informat.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF33 NAT001 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightUL File Number: E157318Appearance: Black and Natural ColorTPCI# 9475101Information provi.. |
|||
Flexural Strength | 221 MPa | 32100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI LNP* Stat-kon* Ultem_UC1200 is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
A. Schulman SCHULAMID® 6 GF15H 30% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
Adell AT-37 Nylon 66, 35% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 758 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy Data provided by the manufacturer, ComAlloy International Company.40% Carbon Fiber Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has b.. |
|||
Flexural Strength | 221 MPa | 32000 psi | IPC TM-650 2.4.4 |
Arlon GenClad™ 280 Low Loss Thermoset Bond-Ply Low loss Ceramic-Filled Thermoset/Thermoplastic Hybrid SystemRivals PTFE laminate electrical performance in a Halogen-Free systemLight weight material relative to standard laminate materialsOptimal .. |
|||
Flexural Strength | 221 MPa | 32000 psi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® NY1GF330 Nylon 6, 33% Glass-Filled 33% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET Information provided by A. Schulman. |