Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 220 MPa | 31900 psi | |
Plastcom SLOVASTER® B GF 40 PBT reinforced with 40% glass fibre Features: PBT for injection moulding, chemically reinforced with 40% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bendi.. |
|||
Flexural Strength | 220 MPa | 31900 psi | ASTM D790 |
Premix Premi-Glas® 1206 LD Fiberglass Reinforced Thermoset SMC Premi-Glas® 1206 LD is a fiberglass reinforced thermoset sheet molding compound for transportation or structural and semi-structural applications where good surface appearance, high strength and du.. |
|||
Flexural Strength | 220 MPa | 31900 psi | ASTM D790 |
NHEP Spectron™ E6666 Nylon 66, 30% Glass Fiber Natural color. E6666 exhibits high rigidity, mechanical strength, and excellent appearance. It is suitable for wide range of applications.Property data measured at room temperature, 50% RH.Informati.. |
|||
Flexural Strength | <= 220 MPa | <= 31900 psi | ISO 178 |
Polykemi AB SCANAMID 66 A53^ F43 Nylon 66, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Flexural Strength | 220 MPa | 31900 psi | ISO 178 |
Ravago Manufacturing Americas Hylon® N1233HL BK Nylon 6/6 Available in North America Filler: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantAuto Specifications: .. |
|||
Flexural Strength | 220 MPa | 31900 psi | ISO 178 |
Nilit FRIANYL B63 H-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 220 - 240 MPa | 31900 - 34800 psi | Injection; ISO 178 |
Raschig Group RESINOL® 87120 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Flexural Strength | 220 MPa | 31900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP PFL38S PA 6 LNP* LUBRICOMP* PFL38S is a compound based on Nylon 6 resin containing 40% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant |
|||
Flexural Strength | 220 MPa | 31900 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2310 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Flexural Strength | 220 MPa | 31900 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2310F PEI 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Flexural Strength | 220 MPa | 31900 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2310R PEI 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Flexural Strength | 220 - 230 MPa | 31900 - 33400 psi | ISO 178 |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFFR-4133 is a 33% glass-reinforced, halogen-free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. Th.. |
|||
Flexural Strength | 220 MPa | 31900 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA 11 (Asia Pacific) LNP* THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing Glass Fiber. |
|||
Flexural Strength | 220 MPa | 31900 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF007ES PA 66 LNP* THERMOCOMP* RF007ES is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Heat Stabilized, Easy Molding. |
|||
Flexural Strength | 220 MPa | 31900 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE006ER PC LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive. |
|||
Flexural Strength | 220 MPa | 31900 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE006ER PC (Asia Pacific) LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Strength | 220 MPa | 31900 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON RV008E PA 66 (Asia Pacific) LNP* VERTON* RV008E is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Strength | 220 MPa | 31900 psi | ISO 178 |
Unitika A1030GFL45 PA6, 45% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Flexural Strength | 220 MPa | 31900 psi | ISO 178-93 |
Wellman Wellamid® GF33-66/6 XE-NBK1 33% Glass Fiber Reinforced Nylon 66/6 Description: Glass Fiber Reinforced Nylon 66/6Information provided by Wellman. |
|||
Flexural Strength | 220 MPa | 31900 psi | ASTM D790 |
Toyobo VYLOPET® EMC132-01 Injection Molding Polyester Resin, Flame Resistant Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo. |
|||
Flexural Strength | 220 MPa | 31900 psi | ASTM D790 |
Toyobo VYLOPET® EMC132-02 Injection Molding Polyester Resin, Flame Resistant Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo. |
|||
Flexural Strength | 220 MPa | 31900 psi | ISO 178 |
Polyplastics Duranex® 3300 Polybutylene Terephthalate (PBT), Standard, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Strength | 220 MPa | 31900 psi | dry; ISO 178 |
DSM EcoPaXX® Q-PG6 PA410-I-GF30 % Glass Reinforced, Impact Modified |
|||
Flexural Strength | 220 MPa | 31900 psi | dry; ISO 178 |
DSM EcoPaXX® Q-X07208 PA410-I-GF30 % Glass Reinforced, Impact Modified |
|||
Flexural Strength | 220 MPa | 31900 psi | ISO 178 |
Azdel AZMET® CM20350 35% continuous random fiber mat / PBT resin matrix AZDEL® CM20350 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a Polybutylene Terephthalate (PBT) resin matrix. This composite material fea.. |
|||
Flexural Strength | 220 MPa | 31900 psi | ISO Data |
BASF Ultradur B 4406 G6 Q717 30% Glass Filled PBT Ultradur B 4406 G6 Q717 is an UL V0 injection molding, PBT grade with 30% glass fiber reinforcement. |