Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 2000 MPa | 290000 psi | 0°; RT |
Greene Tweed Xycomp® 1001-01 PEEK, Carbon Fiber Filled Greene, Tweeds Xycomp® engineered components offer a wider range of benefits than conventional thermoset resin systems because they rely on thermoplastic resins for their matrix. With specific st.. |
|||
Flexural Strength | 2000 MPa | 290000 psi | |
China Tungsten ZK10UF Tungsten Carbide Semi-finishing and finishing of cast-irons and nonferrous metals it's also the unique material of solid carbide tools for holing.Information provided by China Tungsten |
|||
Flexural Strength | 2000 MPa | 290000 psi | |
China Tungsten ZK30 Tungsten Carbide Roughing of marble, plastics as well as non-ferrous metals, copper and aluminum and cast iron.Information provided by China Tungsten |
|||
Flexural Strength | 2000 MPa | 290000 psi | |
China Tungsten ZK40 Tungsten Carbide High in strength and impact resistance, Roughing and strength cutting of cast iron.Information provided by China Tungsten |
|||
Flexural Strength | 2000 MPa | 290000 psi | |
China Tungsten ZM30 Tungsten Carbide High strength in use; capable of resisting high impact load, yet wear resistance comparatively low. Roughing and semi-finishing of refractory steel, manganese steel, stainless steel, etcInformation.. |
|||
Flexural Strength | 2000 MPa | 290000 psi | Rmb. Four point bend testing. 5 mm ø. 5mm/min. Austenitizing temperature: 1250°C Tempering: 3X1 h at 560°C, AC |
Assab Steels ASP 30 Cold Work Steel ASP 30 is a W-Mo-v-Co alloyed PM high speed steel characterized by:High wear resistanceHigh compressive strength at high hardnessGood through hardening propertiesGood toughnessGood dimensional stabi.. |