Flexural Strength 1910 MPa
277000 psi
China Tungsten YT798 Tungsten Carbide
High toughness and high resistance to thermal shock and plastic deformation. Milling of alloy steel, tool alloy steel, manganese steel and stainless steel.Information provided by China Tungsten
Flexural Strength 1910 MPa
277000 psi
China Tungsten YW2A Tungsten Carbide for Cutting Tools
High red hardness and high strength in use, resisting high impact load, A good grade for general purposes, Machining and medium machine of cast irons and problem materials such as refractory steel, ..