Flexural Strength 1890 MPa
274000 psi
China Tungsten YG6X Tungsten Carbide for Cutting Tools
Fine grain WC alloy, wear resistance higher than YG6,strength in use close to YG6,Machining of chilled alloy cast irons and refractory alloy steel or finishing of ordinary cast irons.Information pro..