Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 1800 MPa | 261000 psi | |
China Tungsten YG643 Tungsten Carbide High wear resistance, high resistance to oxidation and to bonding Machining of cast irons, refectory alloys, stainless steel, quenched steel and non-ferrous materialsInformation provided by China Tu.. |
|||
Flexural Strength | 1800 MPa | 261000 psi | |
China Tungsten YT767 Tungsten Carbide High wear resistance and high resistance to plastic deformation Continuous or intermittent cutting of manganese steel and stainless steel.Information provided by China Tungsten |
|||
Flexural Strength | 1800 MPa | 261000 psi | |
China Tungsten YT790 Tungsten Carbide Better, toughness, wear resistance high impact resistance thermal cracking resistance, and plastic deformation resistance for rough turning ,milling and planning of steel, esp. forgings and castings.. |
|||
Flexural Strength | 1800 MPa | 261000 psi | |
China Tungsten ZK20 Tungsten Carbide Roughing and semi-finishing of cast iron. chilled cast iron, low alloy cast iron, non-ferrous metals and non-metallic materials.Information provided by China Tungsten |
|||
Flexural Strength | 1800 - 2100 MPa | 261000 - 305000 psi | |
China Tungsten Z10 Tungsten Carbide for Mining Purposes High wear resistance, for pillar bit drills.Information provided by China Tungsten |
|||
Flexural Strength | 1800 MPa | 261000 psi | |
China Tungsten ZC2 Tungsten Carbide Coated substrate with higher toughness and slightly less wear resistance than ZC1, for semi-finishing and roughing after coating.Information provided by China Tungsten |
|||
Flexural Strength | 1800 MPa | 261000 psi | |
China Tungsten ZM15 Tungsten Carbide High in red hardness and strength in use; capable of resistiting high impact load. Semi-finishing or finishing of refractory steel, manganese steel, austenitic stainless steel, machining of cast i.. |
|||
Flexural Strength | 1800 MPa | 261000 psi | |
China Tungsten ZP20 Tungsten Carbide High in impact resistance and strength in use. Roughing and semi-finishing of steel, cast steel, forgeable cast iron and nodular cast iron.Information provided by China Tungsten |