Mechanical Properties Metric English Comments
Flexural Strength 1730 MPa
251000 psi
China Tungsten ZP10-1 Tungsten Carbide
Excellent in wear resistance, strength in use and red hardness. Semi-finishing and finishing of steel, cast steel, for geable cast iron and continuous nodular cast iron also suitable for copying , t..
Copyright © lookpolymers.com All Rights Reserved