Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Network Polymers NPP Nylon 66G13L Description: NylonInformation provided by Network Polymers Inc. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Niche Polymer PPHG40BK Homopolymer PP, 40% Glass Fiber Filled Information provided by Niche Polymer |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded
( AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer.. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Gharda Chemicals Gafone S 1320GF Polysulfone (PS)
(discontinued **) Characteristics: High Temperature Resistance - Tg 189°C Excellent Clarity Excellent Mechanical & Electrical properties Easy to process Very good Hydrolytic Resistance Applications: Elec.. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU)
(Unverified Data**) Udel GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resi.. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP EX00548C PEI LNP LUBRICOMP* EX00548C is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Clean Compounding System, Wear Resistant. |
|||
Flexural Strength | 148 MPa | 21500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC LNP* Lubricomp* Lexan_LF1520A compound is a 20% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Flexural Strength | 148 MPa | 21500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Asia Pacific) 20% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Techmer ES Electrablend® PA6/6 GF13 SS10 BK 13/10% Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Stainless Steel Reinforcement, 13/10% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation.. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU), Glass Fiber Udel® GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical .. |
|||
Flexural Strength | 148 MPa | 21500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 855 PBT (Europe-Africa-Middle East) VALOX 855 is 15% glass reinforced PBT+PET blend with improved surface appearance. Applications: external housings, steam irons, appliance housings and lighting parts. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D 790 |
SABIC Innovative Plastics Valox® DR48M PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 148 MPa | 21500 psi | ISO 178 |
SABIC Innovative Plastics Valox® V8030CS PBT+PET Glass filled Valox with enhanced surface |
|||
Flexural Strength | 148 MPa | 21500 psi | 0.125 in, injection molded, unannealed; ASTM D790 |
Styron EMERGEâ„¢ 4202-15 MFR Polycarbonate EMERGEâ„¢ PC 4202-15 advanced resin is 20% glass reinforced polycarbonate containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. A.. |
|||
Flexural Strength | 148 MPa | 21500 psi | 0.125 in, injection molded, unannealed; ASTM D790 |
Styron EMERGEâ„¢ 4202-8 MFR Polycarbonate EMERGEâ„¢ PC 4202-8 advanced resin is 20% glass reinforced polycarbonate containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. Ap.. |
|||
Flexural Strength | 148 MPa | 21500 psi | Method I (3 point load), 2.0 mm/min; ISO 178; ASTM D790 |
Styron CALIBREâ„¢ 5201-12 Polycarbonate Resin Overview: CALIBREâ„¢ 5201-12 polycarbonate resin is 20% glass reinforced containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. CALI.. |
|||
Flexural Strength | 148 MPa | 21500 psi | Method I (3 point load), 2.0 mm/min; ISO 178; ASTM D790 |
Styron CALIBREâ„¢ 5201-8 Polycarbonate Resin Overview: CALIBREâ„¢ 5201-8 polycarbonate resin is 20% glass reinforced containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. CALIB.. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Ensinger Tecapeek® XP-90 Compression Molded PEEK Compound, 25% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Adell ER-18 Homopolymer Polypropylene, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 148 MPa @Temperature -40.0 °C |
21500 psi @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® 8253 HS PA6 (Dry) Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased.. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Applied Composites 8072 Polyester SMC Industry Application: TransportationProduct Application: AutomotiveDistinct Features: Zero Shrink, Superior Class A Finish, Improved Impact, Accepts Mold CoatingInformation provided by Applied Compo.. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Applied Composites 120 Polyester SMC Industry Application: ElectricalProduct Application: Transmission ProductDistinct Features: Pigmentable UL 94 V-5, Stable @ 600 Hour QUV Accelerated Weather Testing, Passed 6 Mos. AZ Outdoor Weather.. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
SABIC Innovative Plastics NORYL PX2934 PPE+PS (Asia Pacific) PPE+PS GF20% High Heat Non-FR |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D 790 |
SABIC Innovative Plastics Valox® VC108 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
Adell ER-38 Homopolymer Polypropylene, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |