Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 128 MPa | 18600 psi | |
Plastcom SLOVALEN PH 59 GF 30 PP, 30% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suita.. |
|||
Flexural Strength | 128 MPa | 18600 psi | ASTM D790 |
Premix Premi-Glas® 1201-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1201-20 is a fiberglass reinforced thermoset sheet molding compound for sanitary ware applications such as shower bases and surrounds, bathtubs and vanity tops.Key features and benefits.. |
|||
Flexural Strength | 128 MPa | 18500 psi | ASTM D790 |
Polymer Resources TP-IM-G15 Polybutylene Terephthalate, 15% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 15% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Flexural Strength | 128 MPa | 18500 psi | ASTM D790 |
Polymer Resources TP-IM-G7.5 Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Flexural Strength | 128 MPa | 18600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DFL32P PC LNP* LUBRICOMP* DFL32P is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Exceptional Processing. |
|||
Flexural Strength | 128 MPa | 18600 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® ET-1001 L Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **) AMODEL ET-1001 L resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resistan.. |
|||
Flexural Strength | 128 MPa | 18500 psi | ASTM D790 |
Polymer Resources NY6-M40 Nylon 6, 40% Mineral Filled Nylon 6, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested .. |
|||
Flexural Strength | 128 MPa | 18500 psi | ASTM D790 |
Polymer Resources NY6-M40-[color]-H Nylon 6, 40% Mineral Filled, Heat Stabilized Nylon 6, 40% Mineral Filled, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Flexural Strength | 128 MPa | 18600 psi | ASTM D790 |
LG Chemical IF870S PMMA, General Purpose Grade for Injection Molding Highest flowability of all gradesFeatures: Excellent transparency and eleganceWeather resistance and chemical resistanceSurface hardness and coloring propertySuperior electrical resistance and mecha.. |
|||
Flexural Strength | 128 MPa | 18600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY RF203H PA 66 LNP LUBRILOY* RF203H is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare. |
|||
Flexural Strength | 128 MPa | 18600 psi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK) AvaSpire® AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (.. |
|||
Flexural Strength | 128 MPa | 18600 psi | ASTM D790 |
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU), Glass Fiber Udel® GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical res.. |
|||
Flexural Strength | 128 MPa | 18500 psi | ASTM D790 |
Techmer ES HiFill® ABS GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 128 MPa | 18500 psi | ASTM D790 |
Techmer ES Luriblend® PA6 GF15 TL15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: Heat Stabilized and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Heat Stab.. |
|||
Flexural Strength | 128 MPa | 18500 psi | ASTM D790 |
Techmer ES Plastiblend® TPX-HTN-000CA Availability: North AmericaForms: Pellets Features: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 128 MPa | 18500 psi | ASTM D790 |
Chase Plastics CP Pryme® N333GL (COND, 50% RH) Nylon 6 (Utility Grade), 33% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 128 MPa | 18600 psi | ISO 178 |
Polyplastics Duranex® 7195W Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Strength | 128 MPa | 18500 psi | ASTM D790 |
Ensinger Tecapeek® XP-109 Compression Molded PEEK Compound, 30% Carbon Fiber with 15% PTFE Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Strength | 128 MPa | 18600 psi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 611 Nylon 6, Glass Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.13% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Flexural Strength | 128 MPa | 18500 psi | ASTM D790 |
Techmer ES Plastiblend® ABS/PBT GF15 Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 128 MPa | 18600 psi | ASTM D790 |
LNP ULTEM® JD7904 Polyetherimide
(discontinued **) Forms: PelletsInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.. |
|||
Flexural Strength | 128 MPa | 18600 psi | ASTM D790 |
Resinoid 2018 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Flexural Strength | 128 MPa @Temperature 150 °C |
18600 psi @Temperature 302 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **) Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg.. |