Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 123.6 MPa | 17920 psi | CW; ASTM D790 |
Haysite H208 Polyester, Magnetic Permeable Grade H208 has high magnetic permeability and excellent retention of properties after heat aging at elevated temperatures. This unique combination of properties allows Grade H208 to be used in vari.. |