Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 118.9 MPa | 17250 psi | ASTM D790 |
Nilit Polynil® P200 High Viscosity Nylon 66 Description: High viscosityApplication: Semi-finished and FilmInformation provided by NILIT. |
|||
Flexural Strength | 118.9 MPa | 17250 psi | ASTM D790 |
Nilit Polynil® P230 High Viscosity Nylon 66 Description: Polynil P230 is a high viscosity NYLON 66 (Viscosity number 280 cm³/gr) that was developed for film- and rod extrusion. It has high melt stability and low gel content. It holds various.. |
|||
Flexural Strength | 118.9 MPa | 17250 psi | ASTM D790 |
Nilit Polynil® P240 High Viscosity Nylon 66 Description: Polynil P240 is a high viscosity NYLON 66 (Viscosity number 290 cm³/gr) that was developed for rod and slab extrusion. It has a high melt stability and a low gel content.Key characteri.. |