Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 114 MPa | 16500 psi | X, Y direction; Condition A; ASTM D790 |
Rogers Corporation TMM® TMM3 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Quadrant EPP Duratron® PI D7015G PI Bearing Grade Polyimide (ASTM Product Data Sheet) |
|||
Flexural Strength | <= 114 MPa | <= 16500 psi | ISO 178 |
Polykemi AB SCANMID 6 B12^ NH11L Nylon 6, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Ravago Manufacturing Americas Enviramid™ N2300HL BK Post Consumer Recycle Nylon 6 Heat Stabilized, Lubricated, Black, and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Resinoid 1382 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
PolyOne Edgetek® AS-20GF/000 HI UV NAT Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **)& Description/Features:Glass Fiber ReinforcedHigh ImpactUV StabilizedNaturalUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Fiberfil® J-60/30/E/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 114 MPa | 16500 psi | |
SGL Carbon Group EK 3205 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Flexural Strength | 114 MPa | 16500 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX11411 PC LNP* STAT-KON* DX11411 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON KEP33 Acetal LNP STAT-KON* KEP33 is a compound based on Acetal resin containing 15% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Techmer ES Plaslube® J-50/10/TF/15 BK223 Polycarbonate |
|||
Flexural Strength | 114 MPa | 16500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF VF006U Super Tough Nylon LNP* Thermotuf* VF006U is a compound based on Super Tough Nylon containing Glass Fiber. Characteristics of this grade are High Impact. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Plenco 6990 Phenolic, Briquette, Injection Molded PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM Test |
BASF Ultramid® 8270 HS PA6 (Dry) Ultramid 8270 HS is a thermally modified PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile extrusion, and other applications requi.. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 651 Nylon 6, Mineral Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.35% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
Adell AS-30 Nylon 66, General Purpose Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 631 Nylon 6/6, Glass Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.13% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Flexural Strength | 114 MPa | 16500 psi | ASTM D790 |
PolyOne Edgetek® AT-20GF/000 FDA Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedFDA CapablePolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 114 MPa @Temperature 175 °C |
16500 psi @Temperature 347 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **) Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg.. |