Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 111 MPa | 16100 psi | ASTM D790 |
Plaskolite Optix® CA-81 General Purpose Acrylic Resin Extrusion Grade Pellets. Highest Molecular weight. |
|||
Flexural Strength | 111 MPa | 16100 psi | ASTM D790 |
Plaskolite West Optix® CA-81 General Purpose Acrylic Resin Extrusion Grade Pellets. Highest Molecular weight. |
|||
Flexural Strength | 111 MPa | 16100 psi | ISO 178 |
Nilit FRIANYL A63 HH-FK 1020 Nylon 6.6 for injection molding, 10% glass fiber and 20% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 111 MPa | 16100 psi | |
Quadrant EPP Nylatron® GSM PA 6 + MoS2, cast (ISO Data) Nylatron GSM contains finely divided particles of molybdenum disulphide to enhance its bearing and wear behaviour without impairing the impact and fatigue resistance inherent to unmodified cast nylo.. |
|||
Flexural Strength | 111 MPa @Temperature 150 °C |
16100 psi @Temperature 302 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Flexural Strength | 111 MPa @Temperature 150 °C |
16100 psi @Temperature 302 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include .. |
|||
Flexural Strength | 111 MPa | 16100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DFL42 PC LNP* Lubricomp* DFL-4042 a compound based on Polycarbonate resin containing 10% Glass Fiber, 20% PTFE. Added features include: Internally Lubricated. |
|||
Flexural Strength | 111 MPa | 16100 psi | ASTM D790 |
Glastic BMC SLC-1000 Glass-Reinforced Polyester Data provided by Glastic Corporation.Medium strength, V-0, adjustable shrinkage. |
|||
Flexural Strength | 111 MPa | 16100 psi | 2 mm/min; ISO 178 |
Ineos ABS Lustran® SAN C Injection Molding Grade |
|||
Flexural Strength | 111 MPa @Temperature 150 °C |
16100 psi @Temperature 302 °F |
4; ISO 178 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Flexural Strength | 111 MPa @Temperature 150 °C |
16100 psi @Temperature 302 °F |
4; ISO 178 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
Flexural Strength | 111 MPa | 16100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DFD02EXC PC (Europe-Africa-Middle East) LNP* Stat-kon* DFD02EXC is a compound based on Polycarbonate resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 111 MPa | 16100 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12 (Asia Pacific) LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 111 MPa | 16100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RKN14 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RKN14 is a compound based on Nylon 66 resin containing Mineral, MOS2. |
|||
Flexural Strength | 111 MPa | 16100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX92002 PC (Europe-Africa-Middle East) LNP* Stat-kon* DX92002 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 111 MPa | 16100 psi | ASTM D790 |
SABIC Innovative Plastics Xenoy® X6320 PBT+PC (Asia Pacific) X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality. |
|||
Flexural Strength | 111 MPa | 16100 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12 LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 111 MPa | 16100 psi | ASTM D790 |
Unitika PT-3020 Characteristics: Dimensional accuracy (planarity) Heat resistance Creep resistance and elasticity RigidityInformation provided by Unitika Ltd. |
|||
Flexural Strength | 111 MPa | 16100 psi | ISO 178 |
Unitika TERRAMAC HV-6250H Polylactic Acid (PLA) Foam, Extrusion, blow, and foam sheet grades. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Flexural Strength | 111 MPa | 16100 psi | ASTM D790 |
A. Schulman ComAlloy Lubrilon® 604 Nylon 6/6, PTFE/Molybdenum Disulfide Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Flexural Strength | 111 MPa | 16100 psi | ISO 178 |
Denka TX-100S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Flexural Strength | 111 MPa @Temperature 150 °C |
16100 psi @Temperature 302 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |
|||
Flexural Strength | 111 MPa | 16100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF WF003I PBT (Europe-Africa-Middle East) LNP* Thermotuf* WF003I BLACK is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: High Impact. |