Flexural Strength 11.0 MPa
1600 psi
Quadrant EPP TIVAR® Oil Filled PE-UHMW + oil (ISO Data)
TIVAR Oil Filled is a self-lubricating PE-UHMW material in the real meaning of the word. Next to an enhanced wear resistance, the incorporated and evenly dispersed oil renders this material a consid..
Flexural Strength 11.0 MPa
1600 psi
ISO 178
SABIC Innovative Plastics LNP COLORCOMP R1000S PA 66
LNP COLORCOMP* R1000S is an unfilled Nylon 66. Added features of this material is: Heat Stabilized.
Flexural Strength 11.0 MPa
1600 psi
ISO 178
SABIC Innovative Plastics LNP COLORCOMP R1000SU PA 66
LNP COLORCOMP* R1000SU is an unfilled Nylon 66 resin. Added features include: Heat Stabilized, UV Stabilized.
Flexural Strength 11.0 MPa
1600 psi
ASTM D790M
DSM Somos® 8110 Epoxy Photopolymer  (discontinued **)
DescriptionDSM Somos® 8110 is a high-speed liquid photopolymer that produces flexible, high-impact-strength, accurate parts using stereolithography machines. It has a wide processing latitude and ..
Flexural Strength >= 11.0 MPa
>= 1600 psi
MarkeTech Repton 601 Mullite
Brand 601 features: High porosity-low bulk density.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, e..
Flexural Strength >= 11.0 MPa
>= 1600 psi
MarkeTech Repton EXP 338 Alumina 99.6%
EXP 338 features high porosity.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cyc..
Flexural Strength 11.0 MPa
1600 psi
UCAR Carbon UCAR® PGX Pressure Molded Graphite
Available in low ash monolithic sizes as large as 73" diameter, Grade PGX has excellent erosion resistance and thermal properties.Typical Applications:Fluidized bed reactors Centrifugal casting mold..
Flexural Strength 11.0 MPa
1600 psi
Outer Fiber Stress at 3.5% Outer Fiber Strain; DIN EN ISO 178
Wolf Kunststoff ZEDEX® ZX-100EL55 A1F Polymer Alloy, Elastomer Modified
Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol..
Flexural Strength 11.0 MPa
1600 psi
Olsen; ASTM D747
UBE J5019 Polyethylene
Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope..
Flexural Strength 11.0 MPa
1600 psi
ASTM D790
UBE UBESTA® 3035JU5 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, heat resistanceInformation provided by UBE.
Flexural Strength 11.0 MPa
1600 psi
SAE J949
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness)
AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Strength 11.0 MPa
1600 psi
SAE J949
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness)
AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Copyright © lookpolymers.com All Rights Reserved