Polymer Property : Flexural Strength = 107.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 107.8 MPa
15640 psi
ASTM D790
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6
Information provided by A. Schulman.
Flexural Strength 107.8 MPa
15640 psi
ASTM D790
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6
Information provided by A. Schulman.
Flexural Strength 107.8 MPa
15640 psi
ASTM D790
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6
Information provided by A. Schulman.
Flexural Strength 107.8 MPa
15640 psi
ASTM D790
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6
Information provided by A. Schulman.
Flexural Strength 107.8 MPa
15640 psi
ASTM D790
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6
Information provided by A. Schulman.
Flexural Strength 107.8 MPa
15640 psi
ASTM D790
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6
Information provided by A. Schulman.
Flexural Strength 107.8 MPa
15640 psi
ASTM D790
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6
Information provided by A. Schulman.
Flexural Strength 107.8 MPa
15640 psi
ASTM D790
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6
Information provided by A. Schulman.
Flexural Strength 107.8 MPa
15640 psi
ASTM D790
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6
Information provided by A. Schulman.
Flexural Strength 107.8 MPa
15640 psi
ASTM D790
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6
Information provided by A. Schulman.
Flexural Strength 107.8 MPa
15640 psi
ASTM D790
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6
Information provided by A. Schulman.
Flexural Strength 107.8 MPa
15640 psi
ASTM D790
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6
Information provided by A. Schulman.