Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 102 MPa | 14800 psi | ASTM D-790 |
Plaskolite Optix® CA - 51 KC General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Flexural Strength | 102 MPa | 14800 psi | ASTM D-790 |
Plaskolite Optix® CA - 51 UVT General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Flexural Strength | 102 MPa | 14800 psi | ASTM D790 |
Plaskolite Optix® CA-51 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Medium heat resistance and medium flow. |
|||
Flexural Strength | 102 MPa | 14800 psi | ASTM D-790 |
Plaskolite West Optix® CA - 51 FDA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Flexural Strength | 102 MPa | 14800 psi | ASTM D-790 |
Plaskolite West Optix® CA - 51 UVT General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Flexural Strength | 102 MPa | 14800 psi | ASTM D790 |
Polymer Resources TPSF-FRG10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Flexural Strength | 102 MPa | 14800 psi | ISO 178 |
SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Reta.. |
|||
Flexural Strength | 102 MPa | 14800 psi | ASTM D-790 |
Plaskolite West Optix® CA - 51 HF General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Flexural Strength | 102 MPa | 14800 psi | ASTM D-790 |
Plaskolite West Optix® CA - 51 KC General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Flexural Strength | 102 MPa | 14800 psi | ASTM D-790 |
Plaskolite West Optix® CP - 51 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Flexural Strength | 102 MPa | 14800 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD000 PC (Asia Pacific) LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 102 MPa | 14800 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DD000 PC (Asia Pacific) LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 102 MPa | 14800 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DD0009 PC (Asia Pacific) LNP* Stat-kon* DD0009 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Flexural Strength | 102 MPa | 14800 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DD0009 PC (Europe-Africa-Middle East) LNP* Stat-kon* DD0009 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Flexural Strength | 102 MPa | 14800 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD0009P PC (Asia Pacific) LNP STAT-KON* DD0009P is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 102 MPa | 14800 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DD0009P PC (Asia Pacific) LNP STAT-KON* DD0009P is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 102 MPa | 14800 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC (Europe-Africa-Middle East) LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 102 MPa | 14800 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC (Europe-Africa-Middle East) LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 102 MPa | 14800 psi | ASTM D790 |
Techmer ES HiFill® PBT G/CF30 40% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 102 MPa | 14800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP ZX06323 PPE+HIPS (Asia Pacific) This material is mineral filled PPO grade with high dielectric constant and low loss tangent |
|||
Flexural Strength | 102 MPa | 14800 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing 40% Glass Bead. |
|||
Flexural Strength | 102 MPa | 14800 psi | ASTM D790 |
Plastics Group Polifil® GFABS-10 10% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire.. |
|||
Flexural Strength | 102 MPa | 14800 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1236 Glass Filled Chemically Coupled Homopolymer Polypropylene DescriptionPolyfort® FPP 1236 is a 20% glass filled chemically coupled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 102 MPa | 14800 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1236 Glass Filled Chemically Coupled Homopolymer Polypropylene DescriptionPolyfort® FPP 1236 is a 20% glass filled chemically coupled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 102 MPa | 14800 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1236 Glass Filled Chemically Coupled Homopolymer Polypropylene DescriptionPolyfort® FPP 1236 is a 20% glass filled chemically coupled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 102 MPa | 14800 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1236 Glass Filled Chemically Coupled Homopolymer Polypropylene DescriptionPolyfort® FPP 1236 is a 20% glass filled chemically coupled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 102 MPa | 14800 psi | 0.05 in/min; 3-point; ASTM D790 |
Americas Styrenics STYRON™ 668 General Purpose Polystyrene Resin STYRON™ 668 is a general purpose polystyrene with medium flow and a balance of heat resistance and stiffness characteristics that make it suitable for applications such as CD jewel boxes. STYRON™.. |
|||
Flexural Strength | 102 - 107 MPa | 14800 - 15500 psi | 90 Minute UV Cure; ASTM D790 |
3D Systems Accura® SI 40 Plastic for the SLA® 500 System Accura 40 "Ar" or "Hc" type materials - for the SLA 500 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing .. |
|||
Flexural Strength | 102 MPa | 14800 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WF002I PBT LNP* THERMOTUF* WF006I is a compound based on PBT resin containing 10% Glass Fiber. Added feature of this grade is: High Impact. |