Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 0.350 MPa | 50.8 psi | 48 hour silo aging time |
Jackon JACKOCELL® S3312 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionA substantial reduced pentane emission has been made possible with Jackocell® S3312 - which will lead the industry into the future. High stability of pre-expanded be.. |
|||
Flexural Strength | 0.350 MPa | 50.8 psi | 64 hours silo aging time |
Jackon JACKOCELL® S3312 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionA substantial reduced pentane emission has been made possible with Jackocell® S3312 - which will lead the industry into the future. High stability of pre-expanded be.. |