Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Clash Berg Modulus | 0.689 GPa | 99.9 ksi | ASTM D1043 |
PolyOne Geon™ Vinyl Flexible A75M1 Trans 9000 Polyvinyl Chloride, Flexible (PVC, Flexible) This compound is certified for fuel hose applications(R1 Type B Class 1)under SAE J 1527 requirements.Information provided by PolyOne |