Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Clash Berg Modulus | 0.0241 GPa | 3.50 ksi | ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B65F1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.0241 GPa | 3.50 ksi | ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B6500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Clash Berg Modulus | 0.0241 GPa | 3.50 ksi | ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B65U0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |