Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 13.0 - 17.0 MPa @Strain 100 % |
1890 - 2470 psi @Strain 100 % |
TM-019G |
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM.. |
|||
Tensile Stress | 13.0 - 17.0 MPa @Strain 100 % |
1890 - 2470 psi @Strain 100 % |
TM-019G |
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM.. |