Polymer Property : Tensile Stress = 9501 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 65.51 MPa

@Strain 4.00 %,
Temperature 150 °C
9501 psi

@Strain 4.00 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSRX BK099 a 35% glass reinforced heat stabilized hydrolysis resistant PA66 for injection molding. Developed for applications designed fo..
Tensile Stress 65.51 MPa

@Strain 2.40 %,
Temperature 150 °C
9501 psi

@Strain 2.40 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Zytel HTN52G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin that can be molded in water heated m..