Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 63.15 MPa @Strain 0.560 %, Temperature 23.0 °C |
9159 psi @Strain 0.560 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66