Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 61.83 MPa

@Strain 0.520 %,
Temperature 23.0 °C
8968 psi

@Strain 0.520 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® PLS 95G50DH2 BK261 Nylon 6  (Unverified Data**)
50% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology only from DuPont providing exceptional Heat Resistanc..