Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 61.1 MPa @Strain 4.90 %, Temperature 23.0 °C |
8860 psi @Strain 4.90 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem.. |
|||
Tensile Stress | 61.1 MPa @Strain 2.08 %, Temperature 60.0 °C |
8860 psi @Strain 2.08 %, Temperature 140 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |