Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 59.6 MPa @Strain 4.00 %, Temperature 23.0 °C |
8640 psi @Strain 4.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500P BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved ProcessingDelrin 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin 500P has improved pro.. |
|||
Tensile Stress | 59.6 MPa @Strain 0.710 %, Temperature 0.000 °C |
8640 psi @Strain 0.710 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G33HS1L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin with outstanding impact resistance developed usin.. |
|||
Tensile Stress | 59.6 MPa @Strain 14.4 %, Temperature 40.0 °C |
8640 psi @Strain 14.4 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |