Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 57.1 MPa @Strain 7.70 %, Temperature 40.0 °C |
8280 psi @Strain 7.70 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Tensile Stress | 57.1 MPa @Strain 9.60 %, Temperature 40.0 °C |
8280 psi @Strain 9.60 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500CL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL is a medium viscosity acetal homopolymer resin containing a chemical lubricant designed for low wear and fr.. |
|||
Tensile Stress | 57.1 MPa @Strain 4.21 %, Temperature 150 °C |
8280 psi @Strain 4.21 %, Temperature 302 °F |
ISO 527 |
DuPont Performance Polymers Rynite® FR543 NC010 PET Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm.. |