Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.33 MPa @Strain 300 %, Temperature 23.0 °C |
773 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ HC MT224 Thermoplastic Elastomer (TPE) Versaflex™ HC MT224 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT224 has been specially formulated without the use of any plasticize.. |
|||
Tensile Stress | 5.33 MPa @Strain 300 % |
773 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P3875H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |