Tensile Stress 4.69 MPa

@Strain 300 %
680 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® C4970 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress 4.69 MPa

@Strain 300 %
680 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ XL-2075 Thermoplastic Polyolefin Elastomer (TPO (POE))
PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o..
Tensile Stress 4.69 MPa

@Strain 50.0 %
680 psi

@Strain 50.0 %
ASTM D412
Teknor Apex Monprene® MP-1848K Thermoplastic Elastomer
Uses: Wire and Cable ApplicationsForms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to..