Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.42 MPa @Strain 300 % |
641 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® D6860 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Tensile Stress | 4.42 MPa @Strain 100 % |
641 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P1785 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 4.42 MPa @Strain 1.96 %, Temperature 150 °C |
641 psi @Strain 1.96 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)
(Unverified Data**) Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also.. |
|||
Tensile Stress | 4.42 MPa @Strain 0.0700 %, Temperature 120 °C |
641 psi @Strain 0.0700 %, Temperature 248 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6
(Unverified Data**) Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc.. |