Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 42.0 MPa @Strain 9.50 %, Temperature 40.0 °C |
6090 psi @Strain 9.50 %, Temperature 104 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 42.0 MPa @Strain 12.0 %, Temperature 120 °C |
6090 psi @Strain 12.0 %, Temperature 248 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 42.0 MPa @Strain 1.00 % |
6090 psi @Strain 1.00 % |
|
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, Conditioned Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers.. |
|||
Tensile Stress | 42.0 MPa @Strain 30.0 %, Temperature 80.0 °C |
6090 psi @Strain 30.0 %, Temperature 176 °F |
|
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Tensile Stress | 42.0 MPa @Strain 2.40 %, Temperature 23.0 °C |
6090 psi @Strain 2.40 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani.. |
|||
Tensile Stress | 42.0 MPa @Strain 2.40 %, Temperature 23.0 °C |
6090 psi @Strain 2.40 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b.. |
|||
Tensile Stress | 42.0 MPa @Strain 1.80 %, Temperature 150 °C |
6090 psi @Strain 1.80 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
Tensile Stress | 42.0 MPa @Strain 1.22 %, Temperature 90.0 °C |
6090 psi @Strain 1.22 %, Temperature 194 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 42.0 MPa @Strain 100 % |
6090 psi @Strain 100 % |
ASTM D412 |
Alliance Polymers Zythane™ 6065D Thermoplastic Polyurethane Elastomer Zythane™ 6065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 42.0 MPa @Strain 100 % |
6090 psi @Strain 100 % |
ASTM D412 |
Alliance Polymers Zythane™ 7065D Thermoplastic Polyurethane Elastomer Zythane™ 7065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 42.0 MPa @Strain 2.00 %, Temperature 23.0 °C |
6090 psi @Strain 2.00 %, Temperature 73.4 °F |
ISO 527 |
BASF Ultrason E 3010 PES Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance. |
|||
Tensile Stress | >= 42.0 MPa @Strain 300 % |
>= 6090 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 472D Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Stress | >= 42.0 MPa @Strain 300 % |
>= 6090 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 672D Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Stress | 42.0 MPa @Strain 4.00 %, Temperature 30.0 °C |
6090 psi @Strain 4.00 %, Temperature 86.0 °F |
ISO 527 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |