Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.14 MPa @Strain 300 %, Temperature 23.0 °C |
600 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7431-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7431-1001-00 is an easy processing, performance TPE designed for use in applications requiring a tough, durable material with a low coefficient of friction. - Excellent Heat Stability - .. |
|||
Tensile Stress | 4.14 MPa @Strain 200 % |
600 psi @Strain 200 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ EG-9172 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun.. |
|||
Tensile Stress | 4.14 MPa @Strain 300 % |
600 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Telcar® TL-1336 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Stress | 4.14 MPa @Strain 50.81 %, Temperature 100 °C |
600 psi @Strain 50.81 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process.. |
|||
Tensile Stress | 4.14 MPa @Strain 98.83 %, Temperature 150 °C |
600 psi @Strain 98.83 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |