Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 580 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 4.00 MPa

@Strain 300 %
580 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S FR 60A-3S1846 Thermoplastic Elastomer (TPE)
OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo..
Tensile Stress 4.00 MPa

@Strain 100 %
580 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ U 5370A-S0015 Thermoplastic Elastomer (TPE)
OnFlex™-U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™-U 5300 series are based upon alloys of SEBS and TPU, combining the advantages of..
Tensile Stress 4.00 MPa

@Strain 100 %
580 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P1785D TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 4.00 MPa

@Strain 300 %
580 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ EG-9077 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun..
Tensile Stress 4.00 MPa

@Strain 100 %
580 psi

@Strain 100 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ XL-2075 Thermoplastic Polyolefin Elastomer (TPO (POE))
PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o..
Tensile Stress 4.00 MPa

@Strain 0.196 %,
Time 3.60e+6 sec
580 psi

@Strain 0.196 %,
Time 1000 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66  (Unverified Data**)
20% Glass Reinforced Heat Stabilized Polyamide 66 Developed for Blow Molding Zytel BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Perf..
Tensile Stress 4.00 MPa

@Strain 47.17 %,
Temperature 90.0 °C
580 psi

@Strain 47.17 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers
Tensile Stress 4.00 MPa

@Strain 100 %
580 psi

@Strain 100 %
ASTM D412
Alliance Polymers Zythane™ 4080A Thermoplastic Polyurethane Elastomer
Zythane™ 4080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress 4.00 MPa

@Strain 100 %
580 psi

@Strain 100 %
ASTM D412
Alliance Polymers Zythane™ 5080A Thermoplastic Polyurethane Elastomer
Zythane™ 5080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress 4.00 MPa

@Strain 100 %
580 psi

@Strain 100 %
ASTM D412
Alliance Polymers Zythane™ 6075A Thermoplastic Polyurethane Elastomer
Zythane™ 6075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress 4.00 MPa

@Strain 100 %
580 psi

@Strain 100 %
ASTM D412
Alliance Polymers Zythane™ 6080A Thermoplastic Polyurethane Elastomer
Zythane™ 6080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress 4.00 MPa

@Strain 100 %
580 psi

@Strain 100 %
AorTech Biomaterials Elast-Eon™ E5-130 Biomedical Polyurethane Pellets
Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation.
Tensile Stress 4.00 - 6.00 MPa

@Strain 100 %
580 - 870 psi

@Strain 100 %
TM-019G
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets
Elast-Eon™ 5-325 is a polyurethane with a 32.5% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in ..
Tensile Stress >= 4.00 MPa

@Strain 100 %
>= 580 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 282A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Tensile Stress >= 4.00 MPa

@Strain 100 %
>= 580 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 582A Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Tensile Stress >= 4.00 MPa

@Strain 300 %
>= 580 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 670A Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Stress 4.00 MPa

@Strain 300 %
580 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ P70A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P70A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 4.00 MPa

@Strain 300 %
580 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ P70A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P70A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 4.00 MPa

@Strain 100 %
580 psi

@Strain 100 %
ASTM D412
Alliance Polymers Zythane™ 7080A Thermoplastic Polyurethane Elastomer
Zythane™ 7080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress >= 4.00 MPa

@Strain 300 %
>= 580 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 370A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tensile Stress 4.00 MPa

@Strain 100 %
580 psi

@Strain 100 %
AorTech Biomaterials Elast-Eon™ E5-130 Biomedical Polyurethane Pellets
Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation.
Tensile Stress 4.00 - 6.00 MPa

@Strain 100 %
580 - 870 psi

@Strain 100 %
TM-019G
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets
Elast-Eon™ 5-325 is a polyurethane with a 32.5% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in ..
Tensile Stress 4.00 MPa

@Strain 100 %
580 psi

@Strain 100 %
ASTM D412
Alliance Polymers Zythane™ 7075A Thermoplastic Polyurethane Elastomer
Zythane™ 7075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress >= 4.00 MPa

@Strain 100 %
>= 580 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 782A PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Copyright © lookpolymers.com All Rights Reserved